this post was submitted on 16 Jun 2023
1 points (100.0% liked)

3DPrinting

15583 readers
139 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: !functionalprint@kbin.social or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 1 year ago
MODERATORS
 

If only there was some way I could have known to try this sooner! /s

Story: I wanted to try printing with petg, since I've read how much easier it is. But with a new roll I just had a really hard time. Lots of stringing, poor adhesion, and it just seemed like no amount of my usual fiddling would really make it better.

Somewhere I read that even new filament can benefit from drying, because maybe it wasn't stored in the best way, or maybe it's older than you think. I also read about putting the roll on the print bed, heating it up and covering it for a long time, since I don't have a filament dryer. I did that for about half a day, and then sealed the roll in a ziptop bag with a silica packet because I needed a break from it. A week later and, it seems much better!?

Either the drying, the break, or something else seems to have helped a lot! Happy printing everyone.

you are viewing a single comment's thread
view the rest of the comments
[–] galaxi@lemmy.world 1 points 1 year ago (1 children)

PETG is truly a pain!! You'd think with a plastic used in water bottles, it would do better with moisture. I recommend the brand CC3D if you want something reliable (and ultra cheap!) Also remember that PETG needs more room between the nozzle and the build plate (higher z offset) so that the filament doesn't stick to the nozzle and make a mess :)

[–] boothin@kbin.social 1 points 1 year ago

Think about what happens to water if it's heated above 100C... it turns into steam! The more water there is in the plastic the more steam there will be, causing the various issues like bubbling. The release of steam also means some of the heat is not being absorbed by the filament, leading to temperature issues as it exits the nozzle